Table 2 The Lifshitz–van der waals (γLW) (mJ/m2) and electron-donor (γ) (mJ/m2) and electron-acceptor (γ+) (mJ/m2) parameters of cedar wood surfaces with different roughness

From: Theoretical effect of cedar wood surface roughness on the adhesion of conidia from Penicillium expansum

Ra (μm)

γLW

γ

γ+

Ra = 1.83 (0.09)

46.09 (0.3)

0 (0)

0 (0)

Ra = 1.74 (0.1)

39.77 (0.7)

0.62 (0.4)

0.72 (0)

Ra = 1.5 (0.07)

36.61 (1.3)

1.11 (0.8)

3.90 (1)

Ra = 1.21 (0.05)

48.60 (0.6)

1.71 (0.5)

0.90 (0.7)

Ra = 0.8 (0.03)

43.28 (1)

1.98 (0.9)

2.76 (0.1)

Ra = 0.75 (0.05)

43.62 (0)

10.97 (0.1)

0.29 (1.6)

Ra = 0.6 (0.08)

48.55 (0.1)

9.68 (0.6)

1.06 (1.9)

Ra = 0.45 (0.05)

49.04 (0.2)

10.39 (0.3)

1.30 (1.7)