Skip to main content

Table 1 Percentage of weight loss of LDPE films (values are duplicates and expressed as mean ± standard deviation)

From: Isolation and screening of low-density polyethylene (LDPE) bags degrading bacteria from Addis Ababa municipal solid waste disposal site “Koshe”

Isolates code

Initial weight (g)

Final weight (g)

Percentage of weight loss

KS119

0.2

0.1615

23.87 ± 0.11c

KS114

0.2

0.197

1.25 ± 1.06e

KS16

0.2

0.1999

0.025 ± 0.03536f

KS17

0.2

0.1998

0.05 ± 0.07071f

KS19

0.2

0.196

2.05 ± 1.48e

KS35

0.2

0.1405

42.87 ± 1.91a

KS116

0.2

0.176

13.31 ± 0.46d

KS110

0.2

0.194

2.88 ± 3.36e

KS117

0.2

0.199

0.35 ± 0.21e

KS118

0.2

0.1999

0.025 ± 0.03536f

KS15

0.2

0.198

0.75 ± 0.35e

KS25

0.2

0.196

1.91± 2.42e

KS26

0.2

0.1999

0.025 ± 0.03536f

KS14

0.2

0.1465

37.2 ± 3.06b

Control

0.2

0.2

0

  1. Differences in means are indicated with lowercase letters. Means with same superscript letters are not significantly different, while means with different superscript letters are significantly different (P < 0.05)